International Concrete Abstracts Portal

  


Title: Review and Analysis of FRP Bond Lengths from Pull-out Testing Database with Reduced Embedment Lengths

Author(s): John J. Myers

Publication: Symposium Paper

Volume: 360

Issue:

Appears on pages(s): 21-35

Keywords: Bond performance; Bond strength; Embedment length; Pull-out test; Rebar diameter; Rebar type.

DOI: 10.14359/51740614

Date: 3/1/2024

Abstract:
The American Concrete Institute (ACI) 440.1R-15 Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars linearly reduces the bar stress and thereby pull-out capacity of FRP bars to zero from an embedment length at 20 bar diameters (db) or less. Most experimental research and data examine the development length of various FRP bars at longer, more traditional, embedment lengths. A database was created from select available data in literature to compare to empirical standards. This investigation examines the bond performance of short embedded FRP bars into concrete considering a pull-out failure mode to expand the understanding of short embedded FRP bars into concrete. Based upon the database collected, for the glass fiber-reinforced polymer (GFRP) rebars, the current 440.1R appear quite conservative. For the basalt fiber-reinforced polymer (BFRP) rebar database collected, the current ACI 440.1R-15 provisions appear unconservative for a statistically significant number of the specimen test results within the database. In the case of the carbon fiber-reinforced polymer (CFRP) database, which is quite limited, the data appears to develop considerably less bond strength than the current 440.1R provisions might suggest which requires deeper investigation for the case of short embedment length bonded CFRP bars.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer