Insights into Phase Assemblage in MgO-Al<sub>2</sub>O<sub>3</sub>-(SiO<sub>2</sub>)-CO<sub>2</sub> Systems

International Concrete Abstracts Portal

  


Title: Insights into Phase Assemblage in MgO-Al2O3-(SiO2)-CO2 Systems

Author(s): H. Nguyen, E. Bernard, P. Kinnunen

Publication: Symposium Paper

Volume: 362

Issue:

Appears on pages(s): 733-737

Keywords: hydrotalcite; low-CO2 cement; Mg-Al LDH; thermodynamic modelling

DOI: 10.14359/51742005

Date: 6/17/2024

Abstract:
The decarbonization of the cement industry will require a versatile portfolio of different alternative cements. In contrast to other known and popular alternatives, cement based on MgO-rich hydrates remains an unexplored topic and little is known about the formation and stability of Mg-Al LDH as the main binding phase in a cement. In this work, we report on experimental work on the phase assemblage of MgO-Al2O3-(SiO2)-CO2-H2O system via the hydration of an amorphous magnesium aluminate (AMA) in the presence of different magnesium carbonates and metakaolin. The data reveal that hydrotalcite is the main hydrate of the cement with relatively fast reaction kinetics in which AMA is fully hydrated after 7 days of curing in ambient water. Additionally, a more detailed phase assemblage will be beneficial in the better understanding and in improving the thermodynamic data for the MgO-Al2O3-(SiO2)-CO2-H2O system and of interest to shed light on the long-term stability of this cement.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer