Use of UHPC H-Piles for an Abutment at the Lily River Detour Bridge in Ontario

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of UHPC H-Piles for an Abutment at the Lily River Detour Bridge in Ontario

Author(s): Philip Loh, Sri Sritharan, Kam Ng, Emad Booya, and Don Gardonio

Publication: Symposium Paper

Volume: 363

Issue:

Appears on pages(s): 81-93

Keywords: UHPC, bridge piles, strength, durability, precast, steel shoes

DOI: 10.14359/51742108

Date: 7/1/2024

Abstract:
Through a Change Proposal by Facca Incorporated, the Ontario Ministry of Transportation (MTO) approved the replacement of the as-tendered steel H-piles by newly designed prestressed/precast Ultra-High-Performance Concrete (UHPC) piles for supporting the west abutment of the Lily River Detour Bridge. The 300 mm (~12”) deep UHPC piles were designed and installed at the west abutment based on the previous successful development and testing of a tapered H-shaped pile at Iowa State University. The east abutment, as tendered, was designed to be supported by six steel H-shaped battered piles driven to bedrock. For the west abutment, six UHPC piles were produced and installed using the same batter. Since the site contained occasional boulders and the design intent to drive the piles to bedrock, the UHPC piles were fitted with steel shoes for the first time. All piles were successfully installed to reach the targeted load bearing capacities. After the replacement bridge was constructed, the detour bridge was removed and the UHPC piles were extracted to examine the conditions of the piles. This presentation will provide details of the innovative design of the piles, fabrication and driving of the piles, and lessons learned from analyzing the driving data and removal of the piles. Fellowship and Scholarship recipients. With the help of generous donors from the concrete community, the ACI Foundation awards high-potential undergraduate and graduate students in engineering, construction management, and other appropriate curricula.




  