Title: Optimum Prestress of Tanks with Pinned Base

Author(s): Troels Brøndum-Nielsen

Publication: Structural Journal

Volume: 95

Issue: 1

Appears on pages(s): 3-8

Keywords: circular prestressing; creep properties; prestressed concrete; redistribution of stress;

DOI: 10.14359/521

Date: 1/1/1998

Abstract:
Amin Ghali and Eleanor Elliott presented in their paper an interesting suggestion for prestressing of circular tanks without sliding joints. For many prestressed tanks the following construction procedure is adopted: In order to ensure compressive hoop forces in the wall near the base, the wall is allowed to slide freely in the radial direction during tensioning (free base). After tensioning such displacements are prevented (pinned base). The present paper addresses the problem of prestress of such tanks.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.