Abstract:
This paper is concerned with the structural behavior of reinforced high-strength concrete corbels. The flow of internal forces and the solution of the problem are discussed. A design approach based on strut-and tie models is proposed. The paper presents the results of experimental investigation conducted with reinforced high-strength concrete corbels and give explanation for them by means of the proposed model. At the end it is shown that, when proper main and web reinforcements are provided, the failure by yielding of the main reinforcement can be achiev3ed and that the models originally developed for normal-strength concrete corbels are suitable to those made with high-strength concrete.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer