Title: High-Performance Concrete Lead State Team Activities: Overview

Author(s): M. W. Beacham

Publication: Symposium Paper

Volume: 189

Issue:

Appears on pages(s): 1-8

Keywords: activities; high-strength concrete; technologies

DOI: 10.14359/5842

Date: 1/1/2000

Abstract:
The AASHTO “Task Force on Strategic Highway Research Program (SHRP) Implementation” developed and instituted the Lead State Program in 1996. The mission of the Task Force was to optimize ways in which SHRP technologies could be implemented at the state level. The Task Force understood the benefits of mutual cooperation in sharing resources, working as teams, and collectively implementing the technologies. In order to achieve their mission the Task Force developed the concept of “Lead States Teams”. A “Lead States Team” is a group of states that are willing to take the lead and assist in the implementation of specific, targeted SHRP technologies in which they have interest and have gained some practical experience.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer