International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bond Properties of High-Strength Fiber Reinforced Concrete

Author(s): B. Aarup and B. C. Jensen

Publication: Symposium Paper

Volume: 180

Issue:

Appears on pages(s): 459-472

Keywords: Applications; bond; fiber concrete; fire resistance; high performance; high-strength; joints; silica fume; steel fiber

DOI: 10.14359/5889

Date: 10/1/1998

Abstract:
CRC (Compact Reinforced Composite) is a special concept for high performance concretes, where ductility is achieved through incorporation of a large content of short, stiff and strong steel fibres (6 vol.%). This ductility combined with high strength (150-400 MPa) - and the ability of the small fi-bres to provide an effective reinforcement against even small cracks, makes it possible to obtain exceptional bond properties for deformed reinforcing bars. Results show that full anchorage is achieved with an embedment length of only 5-10 diameters for ribbed bars, which has led to applications in buildings, where CRC is used for in-situ cast joints between pre-cast decks -joints which can transfer full moments with a width of 100 mm. This type of joint, which was used for a university building, has been extensively tested for different loading situations and for behaviour in a standard fire. As the fibre reinforced matrix provides a strong, ductile joint which responds well to dynamic loads it is expected to perform well under seismic loads.




  