Title: New RC Design Guidelines for High-Rise Reinforced Concrete Buildings using High-Strength Materials

Author(s): S. Otani, M. Teshigawara, M. Murakami and T. Okada

Publication: Symposium Paper

Volume: 176

Issue:

Appears on pages(s): 405-422

Keywords: Earthquake-resistant structures; high-strength concrete; reinforced concrete; strength

DOI: 10.14359/5910

Date: 10/1/1998

Abstract:
The increase in the number of high-rise reinforced concrete buildings has accelerated the research on the manufacturing and development of high strength materials. Ministry of Construction, Japanese Government, organized a national research project from 1988 to 1993 for “the Development of Advanced Reinforced Concrete Buildings using High-strength Concrete and Reinforcement.” This paper introduces the earthquake resistant design guidelines developed as a part of this technical project. The scope is limited to the building height of 200 m, the concrete strength of 60 MPa, and the steel strength of 700 MPa.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer