International Concrete Abstracts Portal

  


Title: Adsorption of Naphthalene Sulfonate Superplasticizers by Cement Particles Through Gel Permeation Chromatography

Author(s): G. Ferrari, T. Cerulli, P. Clemente and M. Dragoni

Publication: Symposium Paper

Volume: 173

Issue:

Appears on pages(s): 869-892

Keywords: Adsorption; cements; chromatography; gels; naphthalene; permeability; superplasticizers

DOI: 10.14359/6217

Date: 9/1/1997

Abstract:
In the present paper a new analytical method for measuring the adsorption of naphthalene sulfonate formaldehyde condensate superplasticizers (NSFC) onto cement is described. By this method, based on the application of Gel Permeation Chromatography (GPC), it is possible to estimate the selective adsorption of the different components of these admixtures (P-naphthalene sulfonate, naphthalene disulfonates, polymer fraction). The results indicate that P-naphthalene sulfonate and naphthalene disulfonates are not substantially adsorbed onto the cement particles, independently on the cement used and the dosage of admixture. The polymeric fractions are adsorbed at different extent according to the dosage of superplasticizer and the cement used. Adsorption tests with two NSFC samples of different molecular weight indicate that the high molecular weight polymer fractions are preferably adsorbed over the low molecular weight fractions. The adsorption isotherms of the polymeric fraction of NSFC superplasticizers with different cements indicate that the saturation dosage depends on the chemical composition, the particle size and the specific surface area of the cements. Moreover, these results indicate that the NSFC polymer fraction is totally adsorbed on different cements up to a certain dosage of superplasticizer. This critical value seems to be related with the minimum dosage of superplasticizer to reach the optimum fluidity of cement mixtures. This observation could be put in relation with the preferred adsorption of the higher molecular weight fractions on NSFC, which exhibit a better superplasticizing effect.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer