International Concrete Abstracts Portal

  


Title: The Effect of Moisture on the Physical and Durability Properties of Methyl Methacrylate Polymer Concrete

Author(s): Jack. J. Fontana and Walter Reams

Publication: Symposium Paper

Volume: 89

Issue:

Appears on pages(s): 91-104

Keywords: coarse aggregates; compressive strength; freeze-thaw durability; methyl methacrylate; moisture content; polymer concrete; repairs.

DOI: 10.14359/6244

Date: 12/1/1985

Abstract:
It has been reported by Dr. D. Fowler and others that the presence of water in a polymer concrete mix containing methyl methacrylate monomer reduces the mechanical strength of the composite. With coarse aggregate containing 3 weight percent moisture or higher reduces the compressive strength of a polymer concrete composite by 50 percent or more. This study was undertaken to determine the influence of moisture in the coarse aggregate on the strength and durability of polymer concrete made with a prepackaged two-component methyl methacrylate system developed at Brookhaven National Laboratory for the Federal Highway Administration. The data generated indicates that the compressive strength of “Fabucre te” polymer concrete composites do decay when water saturated coarse aggregates are used. In addition it was found that the use of some silane coupling agents can be used in the polymer concrete composite used in this study to obtain somewhat higher compressive strengths when water saturated coarse aggre-gates are used.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer