International Concrete Abstracts Portal

  


Title: Mechanical Properties of PIC Impregnated and Polymerized Under High Pressure

Author(s): Yu Feixiong and Huang Yiun-yuan

Publication: Symposium Paper

Volume: 89

Issue:

Appears on pages(s): 161-176

Keywords: compressive strength; impregnating; methyl metha-crylate-; microhardness; polymerization; polymer-portland cement-concrete; porosity; pressure.

DOI: 10.14359/6248

Date: 12/1/1985

Abstract:
A PIG of 2400 kg/cm 2 compressive strength is obtained by use of an ordinary cement mortar of 600 kg/cm2 compressive strength (W/C = 0.5, S/C = 2.5 : 1 by wt.) as matrix and MMA as its impregnant with impregnation and thermal catalytic polymerization under high pressure up to 200 atmospheres. Using the same materials, the compressive strength of the PIC obtained with ordinary impregnation is only 1600 kg/cm2. The polymer loadings of the former and the latter PIC are 9.2% and 7.5% respectively. The following contribute to the super-high compressive strength of this PIC: (1) Minimizing the effect of residural air; (2) Overcoming the airblock effect due to ink-bottle-shaped pores during impregnation; (3) Reducing the effect of shrinkage of impregnant during polymerization; and (4) Increasing the interfacial area and adhesive power between matrix and polymer.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer