International Concrete Abstracts Portal

  


Title: Tensile-Splitting Stress Distribution of Partially Polymer-Impregnated Concrete Cylinders

Author(s): M. Kawakami, H. Tokuda, K. Ishizaki, and M. Kagaya

Publication: Symposium Paper

Volume: 89

Issue:

Appears on pages(s): 177-206

Keywords: composite materials; failure mechanisms; impregnating; methyl methacrylate; porosity; polymer-portland cement-concrete; splitting tensile strength; stress analysis; theory of elas-ticity. _

DOI: 10.14359/6249

Date: 12/1/1985

Abstract:
The tensile-splitting stress distribution for partially polymer-impregnated concrete is mathematically predicted from the viewpoint of theory of elasticity, and the results are confirmed by experiments. It is shown that tensile-splitting load to par-tially polymer-impregnated concrete cylinders can be predicted by the proposed failure mode and compressive strength can be adapted to the law of mixtures for composite materials. Furthermore the experimental equation proposed by Knudsen for the relation between strength and porosity for a porous brittle crystal body is examined. The obtained strengths for partially polymer-impreg-nated concrete can be evaluated more exactly than those heretofore in use.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer