Title: Strength Evaluation of the Manotick Bridge Piers

Author(s): Gilbert A. Hartley, Gerhard T. Suter, Heinz Keller, and David C . Marett

Publication: Symposium Paper

Volume: 88

Issue:

Appears on pages(s): 1-22

Keywords: bridge piers; caissons; computer programs; cracking (fracturing); deep beams; evaluation; finite element method; reinforced concrete; stress analysis

DOI: 10.14359/6257

Date: 11/1/1985

Abstract:
A structural investigation of a bridge pier using the finite element method is presented. For the pier, supported on three caissons with loads applied at the top, the structural action is similar to that of a deep beam. The purpose of this investiga-tion is to examine possible causes of existing cracks in the pier. The simplicity of the application and the accessibility of the computer program are emphasized. Once the finite element model is prepared, experimentation is possible with the effects of various loading conditions, all feasible support conditions and the appli-cation of external posttensioning to prevent further cracking and to relieve internal tension stresses during remedial work.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer