Title: Fatigue in Partially Prestressed Concrete Beams

Author(s): A. E. Naaman

Publication: Symposium Paper

Volume: 75

Issue:

Appears on pages(s): 25-46

Keywords: beams (supports); failure; fatigue (materials); fatigue tests; partial prestressing; prestressed concrete; prestressing steels.

DOI: 10.14359/6400

Date: 9/1/1982

Abstract:
ified. Experimental data on the fatigue life of prestressing strands are compared with data on the fatigue life of partially prestressed beams. A close correlation results of a reliability based models of partially prestressed beams in which serviceability and ultimate strength limit states is observed. Global were considered, are presented. They strongly suggest that fatigue in the reinforcement is a controlling limit state that must be seriously accounted for in design.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer