Title: Deflection of Cracked Prestressed Concrete Members

Author(s): Maher K. Tadros and Amin Ghali

Publication: Symposium Paper

Volume: 86

Issue:

Appears on pages(s): 137-166

Keywords: beams (supports); cracking (fracturing); creep properties; deflection; partial prestressing; prestressed concrete; prestress loss; shrinkage; stress relaxation; structural design.

DOI: 10.14359/6429

Date: 8/1/1985

Abstract:
A manual calculation procedure is presented for predic-tion of deflection of partially prestressed beams. Adequate accur-acy is achieved by accounting for the important parameters affecting the deflection: creep and shrinkage of concrete, relaxation of pre-stressed steel, cross section areas and locations of prestressed and nonprestressed steel and cracking at the sections where the tensile strength of concrete is exceeded. Design aids are presented to sim-plify calculation of properties of cracked sections. Numerical exam-ples are included.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer