Abstract:
Brief consideration is given to the uses of a quantitative measure of durability of concrete structural members. A classification scheme of structures, elements, and causes and effects is reviewed by the use of examples. Any quantitative measure of durability of in-situ structural members must be based on data gathered using non-destructive test methods. For any phenomenon such as cracking, corrosion or spalling which influences durability, three factors must be considered, viz. a method of measurement of the phenomenon, the intensity of the phenomenon, and its distribution over the observed area.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer