Title: Measurement of Thickness of Concrete Pavement and Structural Members

Author(s): Toshiaki Takabayashi and Hiroshi lshida

Publication: Symposium Paper

Volume: 82

Issue:

Appears on pages(s): 659-672

Keywords: concrete pavements; nondestructive tests; resonant frequency; thickness; ultrasonic tests.

DOI: 10.14359/6578

Date: 9/1/1984

Abstract:
This paper describes a method of measuring the thickness of pavement concrete and other concrete structural members. A particular feature of this method involves the combined usage of the ultra-sonic pulse and resonance methods to compute the thickness of concrete by measuring the sonic velocity and resonance frequency of concrete.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer