A Contribution to the Evaluation of Fire Compartment Temperatures on the Basis of Heat Balance Calculations

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Contribution to the Evaluation of Fire Compartment Temperatures on the Basis of Heat Balance Calculations

Author(s): Karl Kordina, Ataman Haksever, and Ulrich Schneider

Publication: Symposium Paper

Volume: 80

Issue:

Appears on pages(s): 237-254

Keywords: evaluation; fire resistance; fires; fire tests; thermal properties.

DOI: 10.14359/6592

Date: 7/1/1983

Abstract:
This paper describes the basic concept of a heat balance calculation on the principles of mass and energybalance equations. The most important parameters such as amount and distribution of combustible material, geometry of the fire compartment, thermal properties of the surrounding surfaces and ventilation conditions are all taken into-consideration. It is shown, that the calculation method developed provides good agreement to the temperature development in a fire compartment as measured in a number of tests.




  