Title: Hysteretic Response of Reinforced Concrete- Frames

Author(s): H. Sucuoglu and A. E. Aktan

Publication: Symposium Paper

Volume: 63

Issue:

Appears on pages(s): 153-172

Keywords: beams (supports); collapse; columns (supports); finite element method; frames; hysteresis; lateral pressure; loads (forces); mathematical models; multistory buildings; reinforced concrete; static loads; structural analysis; yield point.

DOI: 10.14359/6650

Date: 8/1/1980

Abstract:
An analytical procedure to generate reinforced concrete plane frame response to reversing static loading is developed. Yield is permitted to occur and spread to crossections which are not predetermined. Response of a 3 story 2 bay frame under reversed lateral load is investigated with particular reference to locations that yield, propagation of yield, beam and column behavior and collapse. To permit the structure prescribe its locations of inelasticity rather than predetermining these regions was observed to be a significant aspect in mathematical modelling.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer