Title: 
            Summary of Research and Design
Philosophy for Bearing Wall Structures
        
        
            Author(s): 
            A. W. Hendry
        
        
            
                Publication: 
                Journal Proceedings
            
            
                Volume: 
                76
            
            
                Issue: 
                6
            
            
                Appears on pages(s): 
                723-738
            
            
                Keywords: 
                bearing walls; collapse; explosions; high-rise buildings; masonry load-bearing walls;multistory buildings; research; structural design.
            
            
                DOI: 
                10.14359/6966
            
        
        
            Date: 
            6/1/1979
        
        
            Abstract:
            Following the Ronan Point accident in 1968 a considerable amount of research work was carried out in the United Kingdom to assess the liability of bearing wall structures to progressive collapse. This included tests on full-size structures and on load-bearing elements. These investigations are summarized in the paper together with a discussion of the measures developed to prevent the occurrence of progressive collapse in bearing wall structures at the design stage.