Abstract:
Results reported cover long-term exposures of test prisms sawed from samples of commercially produced asbestos-cement pipe. The data relates to the specification requirements for such pipe when proposed for service under conditions of exposure to sulfate soil or sulfate water. With the duration of immersion exposure in 2.5 and 5 percent Na2S04 solutions extending to 8 years, the known resistance of autoclaved asbestos-cement pipe cured com-mercially using high pressure steam was confirmed. When stored in sulfate conditions at temperature of either 73 F (23 C) or 100 F (38 C), linear expansion of test prisms for both sources of HPSC pipe after 8 years was less than 0.05 percent but the expansion was excessive for pipe cured under normal conditions.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.