Deflections of Continuous Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Deflections of Continuous Concrete Beams

Author(s): ACI Committee 435

Publication: Journal Proceedings

Volume: 70

Issue: 12

Appears on pages(s): 781-787

Keywords: beams (supports); continuous beams; cracking (fracturing); deflection; flexural strength; reinforced con-crete; structural analysis; structural design; warpage.

DOI: 10.14359/7141

Date: 12/1/1973

Abstract:
This report discusses the necessary considerations and outlines the procedure for a theoretically exact method of computing the deflection of continuous reinforced concrete beams. It describes the approximate methods currently in use and a proposed new method. Each approximate method is compared for accuracy with certain necessary characteristics and also with pertinent test data. Advantages and disadvantages are cited, and the committee’s recommendations are given.




  