International Concrete Abstracts Portal

  


Title: Optimum Design of Prestressed Beams

Author(s): G. G. Goble and W. S. LaPay

Publication: Journal Proceedings

Volume: 68

Issue: 9

Appears on pages(s): 712-718

Keywords: Beams (supports), computer programs, optimi-zation, prestressed concrete, structural design

DOI: 10.14359/7235

Date: 9/1/1971

Abstract:
Presents a method for obtaining the minimum cost design of a prestressed concrete beam, with costs stated in terms of unit costs of the constituent which can be specified by the designer. The influence of a possible design-specification change is studied.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL