International Concrete Abstracts Portal

  


Title: Physical Composition of Hardened Portland Cement Paste

Author(s): Torben C. Hansen

Publication: Journal Proceedings

Volume: 67

Issue: 5

Appears on pages(s): 404-407

Keywords: capillary space; cement pastes; composition (property); curing; hardened paste structure; hydration; physical properties; porosity; portland cements; water-cement ratio.

DOI: 10.14359/7276

Date: 5/1/1970

Abstract:
Formulas are resented from which numerical values for the physical composition of hardened portland cement paste can be determined. These formulas are based on earlier work by Powers. A numerical example is given for an ordinary portland cement paste.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.