Title: Longitudinal Shear Strength of Composite Beams

Author(s): Paul Johnson

Publication: Journal Proceedings

Volume: 67

Issue: 6

Appears on pages(s): 464-466

Keywords: beams (supports) ; bending; composite construction (concrete and steel) ; concrete slabs; reinforced concrete; shear strength; structural design; ultimate strength method.

DOI: 10.14359/7288

Date: 6/1/1970

Abstract:
In the vicinity of the shear connectors, the slab of a composite steel-concrete beam is subjected to a severe combination of longitudinal shear and transverse bending moment. Existing methods for the design of the transverse reinforcement for this region are compared with the results of tests, and a new ultimate strength design method is proposed.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.