Title: Design of Concrete Overlays for Pavements

Author(s): Subcommittee VIII, ACI Committee 325

Publication: Journal Proceedings

Volume: 64

Issue: 8

Appears on pages(s): 470-474

Keywords: bond (reinforced concrete);concrete pavements;concretes;continuously reinforced concrete pavements;highways;joints;maitenance;overlay; pavements;pavements (airport);reinforced concrete;reinforcement;resurfacing; soil mechanics;structural design

DOI: 10.14359/7577

Date: 8/1/1967

Abstract:
This report up-dates the 1958 report and information on bonded concrete resurfacing presents further . Considerationis also given to concrete overlays on flexible pavements. Design procedures which will give dependable results in situations evaluated by mature engineering judgment are presented; however, note is made that they are subject to further refinement.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.