International Concrete Abstracts Portal

  


Title: Multiple Shells of Translation

Author(s): Nabil S. Hadawi and John L. Tanner

Publication: Journal Proceedings

Volume: 63

Issue: 1

Appears on pages(s): 113-126

Keywords: arch;construction;design;formwork;multiple shells;reinforced concrete;shell; translational shell.

DOI: 10.14359/7617

Date: 1/1/1966

Abstract:
Describes the design and construction of a series of translational shells generated by arcs of circles. The shells are organized into modular bays 25 ft square. The 3 in. thick shells are supported on a series of orthogonal multispan arch frames and cover an area of 12,500 sq ft.




  