Time-Dependent Load Transfer in Reinforced Lightweight Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time-Dependent Load Transfer in Reinforced Lightweight Concrete Columns

Author(s): Thomas A. Holm and Joseph Pistrang

Publication: Journal Proceedings

Volume: 63

Issue: 11

Appears on pages(s): 1231-1246

Keywords: aggregate, column, creep, lightweight aggregate, lightweight concrete, reinfoced concrete, research, shrinkage.

DOI: 10.14359/7668

Date: 11/1/1966

Abstract:
Time-dependent strains of an axially loaded, structural size, reinforced lightweight concrete column were observed for 1 year to verify a theoretical method of predicting the load transfer from concrete to reinforcing steel caused by creep and shrinkage. The method, which modifies "classical" equations by considering the interaction between creep and shrinkage, was verified within engineering tolerances. It provides an adequate means of predicting long term column deformations and load transfer using, as a basis, creep and shrinkage data from plain concrete cylinders.




  