International Concrete Abstracts Portal

  


Title: Strength Contribution of a Pozzolan to Contretes

Author(s): Alvaro Lopez Ruiz

Publication: Journal Proceedings

Volume: 62

Issue: 3

Appears on pages(s): 315-326

Keywords: cement, concrete, pozzolan, research, strength

DOI: 10.14359/7696

Date: 3/1/1965

Abstract:
The strength contribution of a pozzolan of volcanic origin in pozzolan-cement concretes with 15 to 35 percent replacements, as a function of the replacement of portland cement by pozzolan, with cements of different qualities was studied. The term strength contribution of a pozzolan, in pozzolan-cement concretes is defined.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.