An Investigation Of The Permeability Of Mass Concrete With Particular Reference To Boulder Dam

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Investigation Of The Permeability Of Mass Concrete With Particular Reference To Boulder Dam

Author(s): Arthur Ruettgers and E. N. Vidal

Publication: Journal Proceedings

Volume: 31

Issue: 3

Appears on pages(s): 382-416

Keywords: none

DOI: 10.14359/8350

Date: 3/1/1935

Abstract:
The permeability investigation reported was made to provide data particularly applicable to the con- ditions at Boulder Dam, that is, for mass concrete exposed to a maximum hydrostatic head of over 700 ft, and made with s ecial cement and 9.in. maximum size aggregate. The paper is comprehensive and includes (I) a description of the testing apparatus and technique, (2) the test results, (3) examples of the practical application of the investi- gational data, (4) a summary of results and con- clusions, and (5) a discussion of the factors con- trolling the flow of water through concrete and the resultant corrosion.




  