Title: Elimination of Flat Plate Punching Failure Mode

Author(s): Carl Erik Broms

Publication: Structural Journal

Volume: 97

Issue: 1

Appears on pages(s): 94-101

Keywords: bent-up bars; building codes; deflection; ductility; flat concrete plates; flexural strength; punching shear; stirrups; structural design; tests.

DOI: 10.14359/838

Date: 1/1/2000

Abstract:
A design concept that eliminates the punching failure mode of flat plates is verified by testing, and design recommendations are given. Only standard reinforcement is used, which is so easy to fabricate and rapid to install that the solution should be suitable as standard practice for ordinary flat plates as well as for such extreme applications as air-raid shelters. The system provides excellent safety against progressive collapse of flat plate buildings, a basic requirement that seems to be overlooked in many current concrete codes. The provisions of the ACI Code 318-95 for two-way shear capacity of slabs are found unsafe for critical sections outside shear reinforcement and presumably also around large columns.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.