Title: Maintaining Concrete Structures

Author(s): Frank W. Capp

Publication: Journal Proceedings

Volume: 32

Issue: 5

Appears on pages(s): 579-592

Keywords: none

DOI: 10.14359/8398

Date: 5/1/1936

Abstract:
Deterioration of concrete structures due to (I) occluded water plus low temperature, (2) corrosion of reinforcing bars, and (3) unanticipated stresses is considered. The maintenance methods to be followed in dealing with the three causes of deterioration are outlined.




  