Investigation of Causes of Delayed Expansion of Concrete in Buck Hydroelectric Plant

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Investigation of Causes of Delayed Expansion of Concrete in Buck Hydroelectric Plant

Author(s): A. A. Levison and Lion Gardiner

Publication: Journal Proceedings

Volume: 37

Issue:

Appears on pages(s): 665-672

Keywords: none

DOI: 10.14359/8581

Date: 6/1/1941

Abstract:
The concrete in Buck Hydroelectric Plant, built in 1912, qave first noticeable evidence of expansion, in 1922. Expansion continued until at date of this writing dimensions had increased by about 1/2 percent, and potential growth remained. No serious expansion was observed in another hydroelectric plant built only 3 miles away at same time with the same cement, but with different coarse aggregate. The Buck coarse aggregate was crushed phyllite (near slate) and the other crushed gneiss. Comparable expansion was ob-served in certain accelerated laboratory tests on concretes made with the Buck aggregate but with modern cements. The laboratory specimens expanded only, where a high alkali cement was used or where alkali was added to a cement. Also, up to the age of I year, specimens expanded only when stored at an accelerating temperature (I IO F in these tests). It is concluded that expansion is due to a reaction between aggregate and alkalis in cement, probably to form sodium or potassium silicate, and that test specimens stored at 70 F will expand in due time.




  