Title: Precast Concrete Pit Sheeting

Author(s): Jacob Field

Publication: Journal Proceedings

Volume: 41

Issue: 4

Appears on pages(s): 441-452

Keywords: none

DOI: 10.14359/8690

Date: 4/1/1945

Abstract:
The development of lightweight concrete slabs in place of wood planks for pit or box sheeting elimi- nates future settlements of underpinned structures when the buried sheeting rots. Practical use has dem- onstrated that concrete planks add little to the cosl of such work. A summary of the history of box sheeting and of the various types used shows the possibilities for the use of concrete in this phase of construction work.




  