Title: Pressurized Epoxy

Author(s): Iuliu S. Herscovici

Publication: Concrete International

Volume: 3

Issue: 10

Appears on pages(s): 35-36

Keywords: embedment; epoxy resins; pressure grouting; pumps; repairs; tools; voids.

DOI:

Date: 10/1/1981

Abstract:
A new tool has been invented to inject pressurized epoxy into gaps that form between embedded steel plates and concrete. its construction and use are described. Pressurized epoxy is used because of the following advantages: early high strength, final strength greater than the concrete, good adhesive bond on both concrete and steel, no bleeding, less preparation time, and minimum workspace required




  