Title: Computational Materials Science on the Internet

Author(s): Edward J. Garboczi and Dale P. Bentz

Publication: Concrete International

Volume: 19

Issue: 12

Appears on pages(s): 26-27

Keywords: cements; computation; concretes; finite element method; materials science; microstructure; transport properties;

DOI:

Date: 12/1/1997

Abstract:
An electronic monograph describing the current state of the computational materials science of concrete has been developed by researchers at the National Institute of Standards and Technology. It is located on the internet at http://ciks.cbt.nist.gov/ and provides over 800 pages of text and hundreds of figures for the reader to learn about this area. This article briefly describes the monograph, its background, intended purposes, and how to use it.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.