Title: Color: A Force in Construction

Author(s): Paul N. Croushore

Publication: Concrete International

Volume: 7

Issue: 11

Appears on pages(s): 43-45

Keywords: aesthetics; architectural concrete; colored concrete; colors (materials); pigments.

DOI:

Date: 11/1/1985

Abstract:
The theme of aesthetics with a purpose is discussed by using examples of existing structures to show how color affects how people feel, act, and think. Background data for architects, designers, and builders includes information on pigments, colors, coloration, concentration, shape and texture, installa-tion, weatherability, efflorescence, maintenance, and color matching. *




  