Abstract:
This report offers guidelines for the development of a quality assurance system for concrete construction projects. The system is intended to permit the user latitude in judgment regarding the owner's needs, the defined quality goals, the importance of the project, the project size and complexity, and the skills of the involved project organizations. The following articl describes the highlights of a report prepared by Committee 121.




  