Title: Splice Strength of High Relative Rib Area Reinforcing Bars

Author(s): David Darwin, Michael L. Tholen, Emmanuel K. Idun, and Jun Zuo

Publication: Structural Journal

Volume: 93

Issue: 1

Appears on pages(s): 95-107

Keywords: bond (concrete to reinforcement); building codes; deformed rein-forcement; lap connections; reinforcing steels; splicing; structural engineering.

DOI: 10.14359/9680

Date: 1/1/1996

Abstract:
This paper describes the testing and analysis of 83 beam-splice specimens containing No. 5, No. 8, and No. 1 1 (16,25, and 36 mm) bars with relative rib areas (ratio of projected rib area normal to bar axis to the product of the nominal bar perimeter and the center-to-center rib spacing) ranging from 0.065 to 0.140. Concretes containing two different coarse aggregates were used to evaluate the effect of aggregate properties on bond strength. Sixty specimens contained uncoated bars with confining transverse reinforcement. Thirteen specimens contained uncoated bars without confining reinforcement, and 10 specimens contained epoxy-coated bars, nine without confining reinforcement and one with confining reinforcement. The tests are analyzed to determine the effect of relative rib area and bar diameter on the increase in bond strength provided by confining reinforcement. The tests also provide a preliminary indication of the effect of high relative rib area on the splice strength of epoxy-coated bars. The splice strength of uncoated reinforcement confined by transverse reinforcement increases with an increase in the relative rib area and the bar diameter of the spliced bars. The increase in splice strength provided by transverse reinforcement increases as the strength of the coarse aggregate increases. The use of reinforcing bars with an average relative rib area of 0.1275, an increase from the average value for conventional bars of 0.0727, can provide up to a 26 percent decrease in splice length compared to conven-tional reinforcement when confining reinforcement is used. The savings obtainable with high relative rib area bars is highest for low covers and bar spacings. Epoxy coating appears to have a less detrimental effect on splice strength for high relative rib area bars than for conventional bars. The results indicate that the maximum development length modification factor used for epoxy-coated reinforcement may be reduced by 20 percent.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.