Title: Push-Out Behavior of Rectangular Concrete-Filled Steel Tubes

Author(s): M. A. Parsley, J. A. Yura, and J. 0. Jirsa

Publication: Symposium Paper

Volume: 196

Issue:

Appears on pages(s): 87-108

Keywords: b o n d ; buildings; columns; composite construction; concrete-filled steel tube; connections; design; shear

DOI: 10.14359/9998

Date: 10/1/2000

Abstract:
A series of push-out tests of rectangular concrete-filled tubular columns (CFT) was recently conducted. The objective of this research program was to identify the shear transfer mechanisms between the infilled concrete and the steel tube and to determine a method for evaluating the capacity of the steel-concrete interface in a CFT column. The experimental variables investigated were the wall slenderness ratio (b/t) of the steel tube and the use of shear tab connections to apply axial load to the steel tube. The results of this study indicated that three mechanisms are responsible for shear transfer along the steel-concrete interface in a push-out specimen: adhesion of the concrete to the steel surface, friction, and wedging of the concrete core. The role of each mechanism in transferring shear between the concrete and steel in the CFT push-out specimen at various stages of load and slip is discussed. Design guidelines for shear transfer in rectangular CFT columns are presented, including a proposed bond strength equation and a recommended strength reduction factor for bond.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer