Synopsis - This specification covers styrene-butadiene Iatex-modified concrete as an overlay on concrete bridge decks. It applies to both new construction and rehabilitation of existing decks. It includes certification requirements of the latex products, storage, handling, surface preparation, mixing, application, and limitations.

DOI:

10.14359/9752


Document: 

JL72-24

Date: 

July 1, 1975

Author(s):

ACI Committee 311

Publication:

Journal Proceedings

Volume:

72

Issue:

7

Abstract:

Presents a guide for the required certification of Level I Inspection technicians and Level II Inspectors performing inspection on nuclear power plants in accordance with Appendix VII of the Joint ACI-ASME Standard "Code for Concrete Reactor Vessels and Containments (ACI 359-74)." The certification of Level II Inspection Engineers is not covered in this report but is found in Appendix VII of ACI 359-74.

DOI:

10.14359/11139


Document: 

JL24-20

Date: 

March 1, 1928

Author(s):

M.A. Arnold

Publication:

Journal Proceedings

Volume:

24

Issue:

3

Abstract:

In this paper I shall endeavor to discuss a problem which has confronted the cast stone industry for a number of years, namely, standard specification.

DOI:

10.14359/15391


Results Per Page 





ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer