ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Showing 1-1 of 1 Abstracts search results
Document:
92-S24
Date:
March 1, 1995
Author(s):
ACI Committee 224
Publication:
Structural Journal
Volume:
92
Issue:
2
Abstract:
This report reviews the state of the art in design, construction, and mainte-nance of joints in concrete structures subjected to a wide variety of use and environmental conditions. In some cases, the option of eliminating joints is considered. Aspects of various joint sealant materials and jointing techniques are discussed. The reader is referred to ACI 504R for a more comprehensive treatment of sealant materials, and to ACI 224R for a broad discussion of the causes and control of cracking in concrete construction. Chapters in the report focus on various types of structures and structural elements with unique characteristics: buildings, bridges slabs on grade, tunnel linings, canal linings, precast concrete pipe, liquid-retaining structures, walls, and mass concrete.
DOI:
10.14359/9656