Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
ACI Global Home Middle East Region Portal Western Europe Region Portal
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Showing 1-5 of 237 Abstracts search results
Document:
SP-363-4
Date:
July 1, 2024
Author(s):
Naveen Saladi, Chandni Balachandran, Robert Spragg, Zachary Haber, and Benjamin Graybeal
Publication:
Symposium Papers
Volume:
363
Abstract:
Corrosion of steel reinforcement is one of the primary contributing factors to bridge deck deterioration. Based on the extent of corrosion, different corrosion mitigation strategies can be used to extend the service life of a bridge deck. Bridge deck overlays are efficient tools in reducing active corrosion. While there are multiple overlay solutions that are commonly deployed, including concrete-based and polymer-based systems, ultra-high performance concrete (UHPC) overlays have gained interest from bridge owners in recent years. Another corrosion mitigation strategy is the application of corrosion-inhibiting chemicals and sealers to a concrete surface to reduce the ingress of deleterious ions. The purpose of this paper is to compare different corrosion mitigation strategies and study the effects of such techniques on the bond between the UHPC overlay and the substrate concrete. UHPC overlays were found to be effective in reducing corrosion rates by more than 50 percent. Sealers and corrosion inhibitors applied to the concrete substrate in combination with placing a UHPC overlay reduced the corrosion rates even further. However, sealers and corrosion inhibitors appeared to negatively affect bond strength, potentially increasing the likelihood of overlay delamination.
DOI:
10.14359/51742107
SP-362_49
June 14, 2024
Parisa Heidari, William Wilson, and Patrice Rivard
362
There is a growing concern regarding the accumulation of marine waste and the negative environmental impacts of cement-based materials. To address these issues, this study explores new possibilities for upcycling marine dredged sediments (MDS) from the Magdalen Islands in Quebec as an alternative to sand, which can be challenging to procure for islands. The characterization of these MDS showed their inert quartz nature. However, by employing packing density optimization methods, it was found that MDS can be effectively used as a partial replacement for sand. The study demonstrates that a 20% volumetric replacement of sand with MDS yields a maximum theoretical packing density of 0.796 and an experimental density of 0.747. The physical and mechanical properties of five mortar mixtures with varying volumetric ratios of MDS to sand from 0 to 50% were evaluated. The findings indicate that increasing the MDS dosage results in a slight reduction of slump flow. However, replacing 20% of the sand with MDS provides the maximum packing density and results in a 12% enhancement in 28-day compressive strength (with a slight increase in bulk electrical resistivity). These results highlight the importance of the development of closely packed granular skeletons in cementitious systems for the development of environmentally friendly alternatives to conventional cement-based materials.
10.14359/51741018
SP-362_27
June 11, 2024
Shizhe Zhang, Jeroen Lenderink, Marc Brito van Zijl, Vincent Twigt, Rob Bleijerveld
The shortage of high-quality fine aggregate as an essential component of concrete has become an emerging worldwide concern for the construction industry. Concrete typically comprises up to 30% fine aggregate, which largely influences the strength and durability of the final product. Therefore, finding suitable substitutes for natural fine aggregate has become an important aspect of current concrete research. In this study, we investigated the suitability of using remediated thermal-treated soil and tar-containing asphalt as secondary raw materials in a self-compacting concrete (SCC) mixture. The remediated materials were used as both (1) fine aggregate replacement to replace all the river sand and (2) partial filler/supplementary cementitious material (SCM) replacement. The modified Andreasen and Andersen (A&A) particle packing model was used to determine the optimal replacement level. Based on the optimal mixture design, the impact of the replacement on the fresh and mechanical properties of SCC was evaluated. Additionally, the pozzolanic reactivity of the fine fraction (<125 μm) within the secondary sand was assessed and compared to that of limestone powder. Our findings confirm that using remediated thermal-treated soil and tar-containing asphalt can produce a more circular, sustainable SCC by replacing high-quality natural sand and limestone filler and reducing the environmental impact of conventional SCC. This study contributes to finding viable alternatives to natural fine aggregate and promotes the use of recycled materials in construction.
The shortage of high-quality fine aggregate as an essential component of concrete has become an emerging worldwide concern for the construction industry. Concrete typically comprises up to 30% fine aggregate, which largely influences the strength and durability of the final product. Therefore, finding suitable substitutes for natural fine aggregate has become an important aspect of current concrete research.
In this study, we investigated the suitability of using remediated thermal-treated soil and tar-containing asphalt as secondary raw materials in a self-compacting concrete (SCC) mixture. The remediated materials were used as both (1) fine aggregate replacement to replace all the river sand and (2) partial filler/supplementary cementitious material (SCM) replacement. The modified Andreasen and Andersen (A&A) particle packing model was used to determine the optimal replacement level. Based on the optimal mixture design, the impact of the replacement on the fresh and mechanical properties of SCC was evaluated. Additionally, the pozzolanic reactivity of the fine fraction (<125 μm) within the secondary sand was assessed and compared to that of limestone powder. Our findings confirm that using remediated thermal-treated soil and tar-containing asphalt can produce a more circular, sustainable SCC by replacing high-quality natural sand and limestone filler and reducing the environmental impact of conventional SCC. This study contributes to finding viable alternatives to natural fine aggregate and promotes the use of recycled materials in construction.
10.14359/51740897
SP-362_23
June 6, 2024
Ameer Hamza Ahmed, Marco Liebscher, Cesare Signorini and Viktor Mechtcherine
This study focuses on the feasibility of replacing fly ash with limestone and calcined clay in strain-hardening cementitious composites (SHCC). Three types of composites were considered: a reference one containing fly ash and the other containing two distinct calcined clays (moderate and high metakaolin content) as supplementary cementitious materials (SCM). Mixtures utilized portland cement (PC) with clinker factors of 0.4 and 0.3, reinforced with 2 vol.% high-density polyethylene (HDPE) fibers. At first, the R3 bound water test was carried out to explicitly assess the reactivity of fly ash and the two calcined clays. Subsequently, the compressive and direct tensile behavior of the SHCCs after 28 days of curing age was evaluated. The results revealed that the SHCCs incorporating calcined clays outperformed their counterpart in terms of compressive strength, tensile strength, and ultimate strain, owing to their high pozzolanic activities, and physical properties, particularly their distinct morphologies. Crack analysis conducted through digital image correlation (DIC) highlighted that the SHCCs with calcined clays established a stronger fiber/matrix interface. In conclusion, this research provides valuable insights into the design of ductile SHCC with novel limestone calcined clay cement (LC3), for enhanced sustainability and cost-effectiveness.
10.14359/51740893
SP358_07
October 1, 2023
Mohammad Raihan Mukhlis, Sohel Rana, and M. Abdur R. Bhuiyan
358
This paper focuses on seismic evaluation of retrofitted curved RC bridge in two phases. In first phase, seismic performance of piers was evaluated by equivalent static method using two performance objectives and by nonlinear dynamic method using a suit of compatible ground motion records. In this regard, demand capacity ratio and residual displacement were evaluated in static method and base shear and deck displacement were evaluated in dynamic method. High damping rubber bearings were used for isolation retrofitting purpose, replacing the elastomeric bearing of the as-built bridge. In second phase, damage state corresponding to large displacements in the bridge components was assessed in terms of component and system fragility curves. The numerical results show that the isolation-retrofitted bridge experiences less base shear force associated with increased deck displacement compared with the as-built bridge having no collapse damage state for considered hazard levels.
10.14359/51740234