Document: 

CI4702El-Tawil

Date: 

February 1, 2025

Author(s):

Sherif El-Tawil, Musawer A. Saqif, William Hazelton, Jon Winckler, and Michael Clark

Publication:

Concrete International

Volume:

47

Issue:

2

Abstract:

Ultra-high-performance concrete (UHPC) is an advanced cementitious composite material with extraordinary mechanical and durability properties. This article discusses the construction of a short-span bridge using UHPC as well as the cost considerations associated with building an entire bridge with UHPC and reflects on lessons learned from the process.


Document: 

SP-363-3

Date: 

July 1, 2024

Author(s):

Megan S. Voss, Daniel Alabi, Raid S. Alrashidi, Taylor A. Rawlinson, Christopher C. Ferraro, H. R. Hamilton, Joel B. Harley, and Kyle A. Riding

Publication:

Symposium Papers

Volume:

363

Abstract:

The movement of ultra-high-performance concrete (UHPC) toward wide scale acceptance within the concrete industry has generated interest in developing improved test methods to provide quality assurance for this material. Most test methods currently used to measure the tensile behavior of ultra-high-performance concrete require specialized testing equipment that is not typically owned by precast or ready-mix production facilities. These test methods provide reliable data for quality assurance of newly developed concrete mixes, but they are impractical as quality-control tests, which would need to be performed for every UHPC placement. This paper presents the development of a simple and inexpensive test to measure tensile strength and ductility for UHPC and serve as a quality-control test. This method was developed from the double-punch test, commonly referred to as the “Barcelona test,” but has been revised to incorporate substantial changes to the loading and data collection requirements to eliminate the need for expensive, specialized equipment. It was determined that the modified test method could produce reliable results using a load-controlled testing procedure with manually recorded data points taken every 0.635 mm (0.025 inches) of vertical displacement for ductile concrete specimens. It was also determined that specimen surface grinding, loading rate, and punch alignment did not significantly influence the test results. However, the fabrication of the specimens, specifically the rate and method at which the molds were filled, had a significant effect on the results. Accordingly, any recommended standardized test method based off of this procedure should have requirements on specimen fabrication.

DOI:

10.14359/51742106


Document: 

SP-363-5

Date: 

July 1, 2024

Author(s):

Philip Loh, Sri Sritharan, Kam Ng, Emad Booya, and Don Gardonio

Publication:

Symposium Papers

Volume:

363

Abstract:

Through a Change Proposal by Facca Incorporated, the Ontario Ministry of Transportation (MTO) approved the replacement of the as-tendered steel H-piles by newly designed prestressed/precast Ultra-High-Performance Concrete (UHPC) piles for supporting the west abutment of the Lily River Detour Bridge. The 300 mm (~12”) deep UHPC piles were designed and installed at the west abutment based on the previous successful development and testing of a tapered H-shaped pile at Iowa State University. The east abutment, as tendered, was designed to be supported by six steel H-shaped battered piles driven to bedrock. For the west abutment, six UHPC piles were produced and installed using the same batter. Since the site contained occasional boulders and the design intent to drive the piles to bedrock, the UHPC piles were fitted with steel shoes for the first time. All piles were successfully installed to reach the targeted load bearing capacities. After the replacement bridge was constructed, the detour bridge was removed and the UHPC piles were extracted to examine the conditions of the piles. This presentation will provide details of the innovative design of the piles, fabrication and driving of the piles, and lessons learned from analyzing the driving data and removal of the piles. Fellowship and Scholarship recipients. With the help of generous donors from the concrete community, the ACI Foundation awards high-potential undergraduate and graduate students in engineering, construction management, and other appropriate curricula.

DOI:

10.14359/51742108


Document: 

SP-363-6

Date: 

July 1, 2024

Author(s):

Kuo-Wei Wen, Manuel Bermudez, and Chung-Chan Hung

Publication:

Symposium Papers

Volume:

363

Abstract:

Ultra-high-performance concrete (UHPC) features tensile strain-hardening behavior and a high compressive strength. Existing studies on the shear behavior of UHPC structural members have been focused on prestressed UHPC girders. More experimental data of the shear behavior of non-prestressed UHPC beams are necessary to quantify the safety margin of shear designs for structures. Moreover, while the UHPC members in most studies did not contain coarse aggregate to strengthen their microstructure, the inclusion of coarse aggregate has been shown to substantially reduce the autogenous shrinkage and enhance the elastic modulus for UHPC materials, which is beneficial for structural applications of UHPC. This study experimentally investigated the shear failure behavior of eighteen non-prestressed rectangular UHPC beams. The experimental variables included the volume fraction of fibers, shear span-to-depth ratio of the beams, and coarse aggregate. The detailed shear failure responses of the UHPC beams were discussed in terms of the damage pattern, shear modulus, shear strength, shear strain, and strain energy. The test results showed that the inclusion of coarse aggregate increased the beam shear strength, and its enhancement became more significant with a higher volume fraction of fibers and a lower shear span-to-depth ratio of the beam. In addition to the experimental investigation, a shear strength model for non-prestressed rectangular UHPC beams that accounts for the interactive effect of the key design parameters was developed. An experimental database of the shear strength of the UHPC beams in existing studies was established to assess the performance of the proposed model. It was shown that the proposed model reasonably predicted the shear strength of the UHPC beams in the database with a higher accuracy and lower scatter compared to the results of existing models.

DOI:

10.14359/51742109


Document: 

SP-363-7

Date: 

July 1, 2024

Author(s):

Kusum Saini and Vasant A. Matsagar

Publication:

Symposium Papers

Volume:

363

Abstract:

Lightweight and high-performance materials have become necessary for infrastructure with advanced construction and performance requirements. One of the major challenges with structures made of these materials is their performance under natural and man-made hazards, such as wind, fire, and blast. Therefore, in this study, the performance of ultra-high-performance concrete (UHPC) and UHPC coated with foamed concrete (UHPC-Foamed) and polyurea (UHPC-Polyurea) is investigated under blast load. A finite element model is developed to assess the behavior of UHPC and coated UHPC panels under far-field and near-field blast scenarios. The constitutive behaviors of UHPC and foamed concrete are considered using the concrete damage plasticity model with respective parameters. The polyurea is modeled as a hyperelastic material with the Mooney-Rivlin model. Moreover, the effectiveness of the additional coatings, i.e., foamed concrete and polyurea, on the blast resistance of each panel is presented. The finding of the study shows that both foamed concrete and polyurea enhance the blast resistance of the UHPC concrete panels. Moreover, a comparison between the blast resistance of UHPC-Foamed and UHPC-Polyurea is conducted under far-field and near-field blast scenarios. Also, the effectiveness of foamed concrete and polyurea coatings with different thicknesses to UHPC panels is assessed under both blast scenarios.

DOI:

10.14359/51742110


12345...>>

Results Per Page 





ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer