International Concrete Abstracts Portal

  


Title: SP-012: Flexural Mechanics of Reinforced Concrete

Author(s): Sponsored by: ASCE, ACI, Univ of FL-College of Engrg, and NSF

Publication: Symposium Paper

Volume: 12

Issue:

Appears on pages(s): 601

Keywords:

DOI: 10.14359/14064

Date: 1/1/1965

Abstract:
SP12 Contains the proceedings of the 1964 International Symposium on Flexural Mechanics of Reinforced Concrete. In addition to providing a more basic understanding of the complex, non-ideal flexural behavior of reinforced concrete, this publication aims to further both immediate and long-range objectives in improving the analytical and statistical basis for the flexural design of reinforced concrete.




  