Title:
Tentative Specficiations, Finish Coat Portland Cement Stucco
Author(s):
Sub-Committee I
Publication:
Journal Proceedings
Volume:
25
Issue:
2
Appears on pages(s):
561-564
Keywords:
none
DOI:
10.14359/15585
Date:
2/1/1929
Abstract:
The present Sub-committee 1 on Stucco of Committee C-3 was appointed in May, 1928, to study recommendations and specifications for the preparation and application of Portland cement stucco.