Title: Placement of Tremie Concrete
Author(s): Ben C. Gerwick, Jr.
Publication: Symposium Paper
Volume: 8
Issue:
Appears on pages(s): 9-20
Keywords:
DOI: 10.14359/16646
Date: 1/1/1964
Abstract: Presents some of the rules and lessons learned from experience, as well as analyzing a few of the difficulties and problems encountered, in the placement of high quality concrete under water by the tremie method.