Title: Studies on Behavior of Concretes Under Irradiation

Author(s): S. Granta and A. Montagnini

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 1163-1172

Keywords: barite; compressive strength; concretes; density (mass/volume); flexural strength; heavyweight concretes; high temperature; irradiation; limestone; modulus of elasticity; mortars (material); neutron source; nuclear reactor containment; nuclear reactors

DOI: 10.14359/18109

Date: 1/1/1972

Abstract:
A report of an experiment on the effects of irradiation on standard and BHT (Portland 730 cement and barytic aggregate) mortars is presented.




  