Title: Point Load Test for Estimation of Concrete Compressive Strength

Author(s): David N. Richardson

Publication: Materials Journal

Volume: 86

Issue: 4

Appears on pages(s): 409-416

Keywords: compressive strength; concretes; loads (forces); mechanical tests; tensile strength; tests; Materials Research

DOI: 10.14359/2189

Date: 7/1/1989

Abstract:
The point-load index is presented as a convenient alternate method for determination of relative strength of concrete or as a method of estimation of concrete compressive strength. The test method is presently accepted in the rock mechanics field but is relatively new to the concrete area. The test is quick, inexpensive, reproducible, and the equipment is portable. The test involves the application of a load via two conical platens across the diametral or axial axis of cores or cylinders. In this study, several test variables were evaluated, including three specimen diameters (50.8, 76.2, and 101.6 mm [2, 3, and 4 in.]) two types of coarse aggregate (river gravel and crushed limestone), two types of diameter (initial and final), and two directions of loading (diametral and axial). A total of 36 mixes was evaluated for over 1000 point-load specimens. It was concluded that there is a strong relationship between point-load index and compressive strength. It is recommended that for compressive strength estimations, each job-mix relationship be individually determined. Two methods of size correction are presented. For most purposes, initial specimen diameter should be used for calculation of the point-load index, and the specimens should be loaded diametrally for testing cast cylinders and cores drilled parallel to concrete "bedding" planes.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer