Title: Toughness-Durability of Glass Fiber Reinforced Concrete Systems

Author(s): S. P. Shah, D. Ludirdja, J. I. Daniel, and B. Mobasher

Publication: Materials Journal

Volume: 85

Issue: 5

Appears on pages(s): 352-360

Keywords: accelerated tests; age; alkalies; concrete panels; ductility; durability; fiber reinforced concretes; glass fibers; portland cements; strength; Materials Research

DOI: 10.14359/2247

Date: 9/1/1988

Abstract:
Glass fiber reinforced concrete (GFRC) panels are increasingly being used by the precast industry for cladding panels of new construction and for retrofit projects (1987 volume: 100 million dollars). The widespread development of GFRC has resulted from the development of alkali-resistant glass fibers that have an improved resistance to the alkaline environment that exists in portland cement-based matrices. In spite of the improved alkali resistance, long-term weathering tests reveal that GFRC panels may exhibit reduced tensile strength and a loss of ductility with aging. The strength reduction is currently explicitly accounted for in design recommendations. The significantly reduced strain capacity is not always properly accounted for. This is partly because sufficient information on long-term ductility is not available, and it is difficult to accurately measure and rationally define ductility. It is likely that for many applications of GFRC, their ductility is at least as important as strength (e.g., connections, differential movements) in determining their service lives. This review paper addresses some aspects of long-term ductility of GFRC systems.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer